The Original Prusa magnetic heatbed is designed to hold a removable double-sided flexible spring-steel sheet, designed specifically for easy removal of printed objects from the print surface.

PP steel sheetThe underside of a printed object

The PP sheet is made for printing polypropylene (PP) since its adhesion to standard PEI sheets is generally very poor. The sheet comes with a matt texture, similar to the satin steel sheet with a PEI surface. The sheet is compatible with most polypropylenes, PLA, PETG and TPU, other materials may have insufficient adhesion and should be printed on our standard PEI sheets.

Main attributes

  • Compatible with many types of polypropylene
  • Made for printing without using a glue stick, PP tape and other means of increasing adhesion
  • Slightly textured surface
  • Double-sided! Both sides can be used repeatedly
  • Easy maintenance and good adhesion qualities

Considerations

  • Never clean the PP sheet with acetone! This will damage the surface.
  • For good adhesion properties and easy print removal, clean the print surface with IPA before every printing, just as described in 3D printing handbook.
  • Check the proper first layer height! If the Live Z value is too low and the first layer is too squeezed, print removal may be difficult and may damage the sheet.
  • Some types of polypropylene may be prone to warping and require using brim or are suitable only for printing small parts and models with sparse infill.
  • Keep the sheet as clean as possible! Any grease stain will decrease adhesion.
  • Live Z value needs to be readjusted if you switch sheets. See Perfiles de plancha de acero.
  • Not scratch-resistant!!! Do not use metal spatulas with sharp edges to remove the prints. Be extremely careful when removing the print.
  • Printing with Brim is recommended.
Consumable parts, such as print sheets (satin, smooth, textured, etc.) are not covered by warranty as the coatings will diminish over time. Unless failure has occurred due to a defect in materials or workmanship, cosmetic damage, including but not limited to scratches, dents, cracks, or other cosmetic damage is also not covered by the warranty. Only defective sheets on arrival are covered by warranty.

Maintenance

  • Attracts fingerprints - A good indication of where your sheet is dirty/greasy and that you need to clean it.
  • Clean with ~90% IPA when the sheet is cold. If ~90% IPA is not sufficient, clean with dishwasher soap. Do not leave the sheet wet! It has an anti-corrosion layer but is still not recommended.
  • Never clean with acetone! It might cause damage to the sheet.
  • Some types of paper towels may leave traces on the sheet (fiber pieces).

Filaments

We have done a lot of testing and compiled our results for you to use. To easily see how to prepare your sheet for any filament type, please see our Material table.

Prints don’t stick

If your print surface is perfectly clean and all grease has been removed by wiping it with a paper towel soaked in isopropyl alcohol ~90% and if the first layer height is set up perfectly, yet your print still does not adhere reliably to the print surface, check out Problemas en la primera capa.

Keep in mind that polypropylenes in general tend to warp more than other materials. Sometimes warping may be so strong that larger models (or with dense infill) detach from the surface even over the best surface adhesion. If you experience such strong warping, we recommend using another type of PP for selected print - for example, our Prusament PP Carbon Fiber shows almost no warping at all. You can find more in the articles about polypropylene and warping.

Notes

After removing the 3D-printed object, you may notice a visible imprint on the sheet’s surface. This is only a visual change: it doesn’t leave any marks on the next 3D-printed parts and does not affect the printing properties in any way. Therefore it’s not considered a reason for a warranty claim.

As a result of the temperatures to which the sheet is exposed during printing, some parts on the bottom surface, which is in direct contact with heatbed, may become slightly glossier or with a different shade. This visual change does not adversely affect the printing properties and is also not considered a reason for a warranty claim.

Example of visible imprintImprinted purge lineShade change caused by heatbed

¿Fue útil este artículo?

Comentarios

¿Todavía tienes preguntas?

¿Todavía tienes preguntas?

Si tienes alguna pregunta sobre algo que no se ha tratado aquí, comprueba nuestros recursos adicionales.
Y si eso no lo soluciona, puedes enviar una petición a [email protected] o mediante el botón que hay más abajo.

Contacta con nosotros